The effect of Gd addition on the kinetics of α₂→γ transformation in γ-TiAl based alloys. Ti-47.1Al-1.8Nb-0.5Zr-0.3
V-0.001Gd (0.001Gd) and Ti-46.9Al-1.6Nb-0.5Zr-0.5
V-0.03Gd (0.03Gd) alloys
Deformation behavior and microstructure evolution of a TiB-reinforced Ti-6.5Al-2Zr-1Mo-1V matrix compositeOzerov, M.,
Stepanov, N.,
Sokolovsky, V.,
Astakhov, I.,
Klimova, M.,
Galtsev, A.,
Zherebtsov, S. A Ti-6.5Al-2Zr-1Mo-1
V/TiB metal-matrix composite with 10.0 vol.% of TiB reinforcing fibers
Hot deformation behavior and processing maps of B and Gd containing β- solidified TiAl based alloy-cast β-solidified Ti-43.2Al-1.9
V-1.1Nb-1.0Zr-0.2Gd-0.2B (at.%) alloy were studied. Phase transformation
Successive processes at quarry waste dumps of various ages - Inguletsky and
Sokolovsky - higher pH values were recorded. The basal soil respiration rate of the Kuzbass